1. Introduction:
It is used primarily for testing highly elastic, soft, elastic specimens: plastics and elastomers, films, rubber, etc. with a tensile force of 5 kN.
Opening and closing is carried out by means of a lever. The spring pretension holds the grip open for specimen placement, the scissor effect creates a prestressing force at the start of the test. Thanks to the scissor principle, an automatic clamping occurs with increasing tensile force – an advantage for specimens that narrow during the test.
Clamping jaws have a smooth or serrated surface.
The grip is ideal for tear and peel testing as a top grip.
2. Specification:
Max. tensile load, kN |
5 |
Sample width, mm |
50 |
Opening size, mm |
From 0 to 19 |
Jaw size, mm |
20×50 |
Overall dimensions, mm |
173×130×55 |
For more information on how Hualong can help your company profit through testing, please Click the button.